This study examines the role of oxide composition on the general and localized corrosion of Fe₃₂Ni₃₆Cr₁₄P₆, Metglass 2826A, in acidic 0.1 M NaCl + 0.1 M Na2$04. The general corrosion behaviour of Metglass 2826A was assessed by cyclic potentiodynamic anodic polarization and compared with the behaviour of pure Fe, Ni, Cr and a commercial 304 stainless steel. The pitting corrosion resistance of Metglass 2826A was evaluated by potentiostatic anodic polarization and pit propagation rate testing and compared to the pitting resistance of 304 stainless steel. The degree of interfacial corrosion of crystallized Metglass 2826A was also assessed by electrochemical potentiokinetic reactivation testing and compared to intergranular attack in heat treated 304 stainless steel.
Investigation of the effect of surface finish and heat treatment on the corrosion susceptibility of Metglass 2826A was performed. The general corrosion resistance of Metglass 2826A was improved by polishing compared to the non-roller-contact side of the as-received ribbon. Polishing increased the threshold potential for pit nucleation but decreased the resistance to pit growth. AES analysis revealed polishing reduced the amount of Fe, Cr, Ni, P and S and increased the concentration of B in the passive film.. Polishing of 2826A produced spontaneous passivity and the lack of initial anodic dissolution prevented the incorporation of beneficial species (Cr,P)- in the passive film.
Heat treatments, consisting of two subcritical anneals (SC1, SC2), a high temperature crystallization anneal(MP), and a low temperature crystallization anneal(SS) were performed... SC1, SC2 and MP anneals decreased the general corrosion resistance relative to polished Metglass 2826A. However, low temperature crystallization SS anneal produced the highest general corrosion resistance observed: Pitting current densities for nucleation and growth were lowered- for all heat treatments compared to polished Matglass 2826A. Ranking of the corrosion resistance was correlated with the partitioning of elemental species by AES analysis and through the definition of interaction parameters. Important elemental interactions include Ni-P, Fe-Ni, C-BN1-B and P-B which varied with heat treatment applied potential and the consideration of a 50 A wide interface between the oxide and the base glass.
Crystalline iron and chromium do not display passivity in acidic 0.1 M NaCl 0.1 M Na2 504 Only pure Nt undergoes an active-passive-transpassive transition in this electrolyte. All of these materials showed. poorer corrosion resistance than as-received or polished Metglass 2826A. Crystalling 304 stainless steel showed comparable general corrosion resistance to 2826A. A lower threshold for pit nucleation and higher pitting current densities were observed for 304 stainless steel compared to as-received or polished Metglass 2826A because of the structurally related pitting observed in 304 stainless steel.
Interfacial corrosion of heat treated 304 stainless steel in the active-passive region increased in the order solution treated; stabilized and sensitized. MP annealed 2826A displayed much Higher interfacial corrosion that even sensitized 304 stainless steel because of the enhanced susceptibility of the Cr depleted MS-1 phase. The level of attack was reduced by SS annealing to that observed for solution treated 304 stainless steel because of a refining of the distribution and type of phases present and the increased repassivation ability of the Cr enriched film formed on SS annealed Metglass 2826A.